Quality & Testing Technician - Intermediate

How many salt spray hours? NSS or CASS for your spec | QLQ

The question every buyer asks

Misconception: the "12h vs 96h" debate has never been about the number — it's about your plating type and the acceptance clause.

This page answers How many salt spray hours? NSS or CASS for your spec — a top recurring question from real QLQ customers — with the line-level detail our technicians actually use. Parameters are industry-standard starting ranges; confirm against your supplier TDS.

How many salt spray hours? NSS or CASS for your spec - QLQ workshop photo
QLQ workshop — QLQ workshop photo

Reference table

PlatingRecommendedMisuse risk
Zinc-platedNSS 24–96h"equivalent" CASS conversion → two incompatible judgements
Nickel/chrome decorativeCASS/AASS 16–48hpassing NSS hours off as CASS
High-strength steelNSS + hydrogen-embrittlement reviewsalt spray only → fracture risk
How many salt spray hours? NSS or CASS for your spec - QLQ workshop photo
Process close-up — QLQ workshop photo

How we handle it on the line

  • Blue-white zinc 12–96h, nickel 96–240h are all normal tiers; comparing hours across plating types is invalid communication.
  • Definitions: NSS neutral salt spray (5% NaCl, 35℃, 20°±5° mounting); AASS acidic; CASS acidic + copper salt (faster, for decorative layers); tier range 16/24/48/72/96/168/240/480/720h.
  • Options: three questions set the duration — what does the acceptance clause say; the destination country's customary tier; the real corrosion environment (sea freight, coast, chemical zones).
  • QLQ's quotations list "plating type – test method – hour tier" as three columns, and post-test cleaning/drying follows the standard and is noted in the report.
  • Ask for complete drawing callouts: plating type + thickness + test method + duration + pass criteria (white/red rust).
  • Miss any one and low quotes will exploit it.

Honest boundaries

  • Honest boundary: neutral spray must not be replaced by "shorter acidic equivalents" in formal acceptance — the industry rule-of-thumb is for rough estimation only.
  • Next step: send the acceptance clause text; QLQ returns the test plan and tier-based quotation.

FAQ

Can QLQ provide test reports with the delivery?
Yes — salt spray, thickness and adhesion reports are attached per lot on request.
Can QLQ provide test reports with the delivery?
Yes — salt spray, thickness and adhesion reports are attached per lot on request.
Can QLQ provide test reports with the delivery?
Yes — salt spray, thickness and adhesion reports are attached per lot on request.
Previous Post
Can salt spray hours translate into service years? | QLQ
Next Post
Nickel plating thickness vs salt spray hours: the real chart | QLQ