Scope of this guide

Management version: this defect as cost and risk — the metrics, audit points and claim defence.

Series: finishing.com recurring questions answered with platingclub line practice. Parameters are industry-standard starting ranges — confirm against your supplier TDS.

Triage: symptom → confirm → first move

SymptomLikely rootConfirm byFirst move
Peels in sheets, bare steel showsSurface contamination pre-plateWater-break + peel mapPre-clean audit before dosing
Blisters after bakeHydrogen entry + baking missedBake log vs specEnforce bake window per spec
Adhesion fails on high carbon steelSubstrate-specific prep neededBy-alloy patternStronger activate for that alloy
Peel at edges after storagePost-dip/rinse contaminationStorage test samplesRinse quality check
Random scattered failuresCleaner bath exhaustedCleaner titration logRebalance or dump per trend

Cost, metrics and defence

Cost lineDriverMetricLever
ClaimsPeel in fieldPPM by customerBend gate per load
ScrapLate detection at assemblyAdhesion audit failureSample plan by load
ChemicalsCleaner dumped late/earlyTitration log completenessDump on trend
DelayQuarantine loopsDays in quarantineBake log compliance

Engineer notes

  • One variable per corrective action; verify with the confirm-by column.
  • Records beat memory: log every trial on the tank card.
  • Two failed actions in a row is a senior call — escalate with your log.
Safety: alkaline zinc baths are caustic and hydrogen from pickled steel can ignite. Caustic-rated PPE, no flames near freshly pickled loads, eyewash at the line.

FAQ

Which KPI predicts peel claims?
Cleaner titration compliance and bake log completeness; both drift before claims arrive.
Is 100% adhesion testing worth it?
Sampling per load catches systemic peel; 100% only while a supplier or bath is failing.
What does a peel claim cost vs the gate?
Claims cost freight, credit and trust; the bend gate costs minutes and paper.