Resin Dripping - Junior

Resin Mixing Ratio And Debubble Basics | Resin Dripping Junior Guide

Scope of this guide

This junior-level guide sticks to the basics you must run without help: safe settings, daily checks and the pass criteria you can verify yourself.

Process: Resin Dripping. Figures in this guide are industry-standard starting ranges; confirm against your supplier TDS before locking settings.

Working ranges and control points

The table below is the daily reference for a dripping station. Set by the card, verify by the control point column.

ParameterTypical rangeControl pointWatch out
Mix ratioBy resin kit (A:B)Scale 0.1 g accuracyOff-ratio never cures fully
DegassingVacuum 2–5 min after mixNo visible bubblesSkipped step craters
Pot life20–60 min by kitDiscard at pot endThickened resin traps bubbles
Cure40–60 °C × 60–120 minProfile per thicknessThick pour exotherms
Bubble count QC0 visible > 0.3 mmLight table per batchCold resin is viscous

Standard routine

  1. Warm resin to 25–30 °C for flow
  2. Scale A and B exactly; stir slowly 2–3 min
  3. Degas before pouring, not after
  4. Pour centre-out to let self-level
  5. Cure with profile, log oven load
Resin Dripping junior - Live line operation - QLQ workshop photo
Live line operation — QLQ workshop photo

Engineer notes

  • Stir fast and you whip bubbles in — slow folding wins
  • Pot life shortens in summer; batch smaller
  • Thick pours need stepped cure to avoid exotherm yellowing
  • Dust-free covers over racks during gel
  • Yellowing traces to over-heat or aged hardener
Safety: Uncured resin and hardener are skin sensitisers. Nitrile gloves, no latex, and barrier cream; ventilate the curing oven.
Resin Dripping junior - Close-up of the working zone - QLQ workshop photo
Close-up of the working zone — QLQ workshop photo

FAQ

Why do bubbles keep appearing after degassing?
Cold resin or over-fast stirring. Warm components and fold slowly; degas again if needed.
Can I speed cure with more hardener?
No — off-ratio leaves uncured resin. Follow kit ratio and raise temperature instead.
Why does the surface stay tacky?
Off-ratio mix or expired pot life. Scale exactly and mix fresh within pot life.