Lakierowanie bez pieca — Zarządzanie

Cold Paint Batch Color Standard Book | Cold Painting Management Guide

Scope of this guide

This management guide translates the process into cost, risk and throughput: what to measure, what to audit and where the money leaks.

Process: Cold Painting. Figures in this guide are industry-standard starting ranges; confirm against your supplier TDS before locking settings.

Working ranges and control points

The table below is the daily reference for a cold spray bench. Set by the card, verify by the control point column.

ParameterTypical rangeControl pointWatch out
Thinner ratio5–15% by volumeViscosity cup per batchOver-thin low build
Air pressure2.5–4 barRegulator lockedHigh pressure overspray
Coat count2–3 light coatsDry-touch between coatsHeavy single coat sags
Dry time, ambient20–40 min per coatFinger-drag testStacking too early prints
Colour checkStandard card under D65 + A lightMetamerism screenMatch fails indoors only

Run It As A Business: the management view

Beyond the basic card, this is the layer that matters at your level:

Cost lineWhat drives itMetric to trackTypical lever
ChemicalsDrag-out and bath dumpsCost per 1000 partsRinse counter-flow, drip bars
ReworkFirst-pass yield lossesFPY by defect familyFix top family first
EnergyHeated tanks and idle timekWh per 1000 partsCovers, night setback
ClaimsEscape ratePPM by customerShip gate on FPY

Standard routine

  1. Match colour under two light sources before production
  2. Filter paint through 120 mesh
  3. Keep bench drafts off while spraying
  4. Dry-touch between coats, full dry before pack
  5. Sign the colour standard card per batch
Cold Painting management - Live line operation - QLQ workshop photo
Live line operation — QLQ workshop photo

Engineer notes

  • Metamerism is the classic cold-paint reject — check under shop and daylight lamps
  • Cold booths need warmer thinner ratio in winter
  • Small parts on wire stands show shadow lines — rotate stands 180° between coats
  • Record batch numbers; colour claims trace to them
  • Old paint absorbs moisture — filter twice and test on scrap
Safety: Spray mists carry isocyanates in some 2K paints. Use supplied-air or A2P respirators for 2K products; skin contact needs barrier cream.
Cold Painting management - Close-up of the working zone - QLQ workshop photo
Close-up of the working zone — QLQ workshop photo

FAQ

Why does colour match in the booth but fail at the customer?
Metamerism. Approve colour under both D65 and warm light before production.
Can I speed drying with heat?
Mild warmth 40 °C is fine; hot air skins the coat and traps solvent.
How much thinner should I add?
To viscosity, not volume: target the cup seconds on the paint card, 16–22 s typical.
Which single metric should I start reporting weekly?
First-pass yield by defect family; it exposes rework cost and points at the largest lever.
Resin Mixing Ratio And Debubble Basics | Resin Dripping Junior Guide
Cold Paint Layer Adhesion Data | Cold Painting Senior Guide