Rack Painting - Management

Paint Line First Pass Yield Tracking | Rack (Hanger) Painting Management Guide

Scope of this guide

This management guide translates the process into cost, risk and throughput: what to measure, what to audit and where the money leaks.

Process: Rack (Hanger) Painting. Figures in this guide are industry-standard starting ranges; confirm against your supplier TDS before locking settings.

Working ranges and control points

The table below is the daily reference for a spray line. Set by the card, verify by the control point column.

ParameterTypical rangeControl pointWatch out
Viscosity (Ford cup 4)16–22 sAdjust with thinner by tempToo thin sags on vertical faces
Gun distance150–200 mmOverlap 50% passesClose gun blows wet film
Flash-off5–10 min ambientTack-free before bakeTrapped solvent bubbles
Wet film per pass20–35 µmTwo passes typicalOne heavy pass sags
BakeObject 60–80 °C × 30 minData logger per batchOver-bake embrittles

Run It As A Business: the management view

Beyond the basic card, this is the layer that matters at your level:

Cost lineWhat drives itMetric to trackTypical lever
ChemicalsDrag-out and bath dumpsCost per 1000 partsRinse counter-flow, drip bars
ReworkFirst-pass yield lossesFPY by defect familyFix top family first
EnergyHeated tanks and idle timekWh per 1000 partsCovers, night setback
ClaimsEscape ratePPM by customerShip gate on FPY

Standard routine

  1. Strain paint before loading the cup
  2. Mask contact points and assembly faces
  3. Spray top faces first, verticals last
  4. Hold tack test before parts enter bake
  5. Log viscosity and thinner ratio per batch
Rack (Hanger) Painting management - Live line operation - QLQ workshop photo
Live line operation — QLQ workshop photo

Engineer notes

  • Sag on verticals is viscosity and pass weight, not gun distance alone
  • Masking paper must be heat grade or it sticks in bake
  • Colour drift between batches: strain and mix full kits only
  • Hanger tips touch wet film — rotate hanger bars by shift
  • Flash-off time doubles in humid season
Safety: Solvent vapours are flammable and a health hazard. Ventilate the booth, wear an organic-vapour respirator, and ground guns to prevent static.
Rack (Hanger) Painting management - Close-up of the working zone - QLQ workshop photo
Close-up of the working zone — QLQ workshop photo

FAQ

Why do runs start at part bottoms?
Film build on verticals exceeds sag resistance. Cut viscosity or split into lighter passes.
How long between coats?
Tack-free time, typically 5–10 minutes ambient; longer when humid.
Why does paint lift at contact points?
Masking failed or hanger contact was oily. Clean contacts and re-mask with heat-grade tape.
Which single metric should I start reporting weekly?
First-pass yield by defect family; it exposes rework cost and points at the largest lever.