The question every buyer asks

Misconception: "guaranteed 3 months of color, actually 1 month, and the factory says it depends on personal use" — the root of this classic cross-border saga is that "color-retention months" has no standard definition; factories promise what they cannot verify.

This page answers Supplier promised 3-month color retention, got 1 month — a top recurring question from real QLQ customers — with the line-level detail our technicians actually use. Parameters are industry-standard starting ranges; confirm against your supplier TDS.

Supplier promised 3-month color retention, got 1 month - QLQ workshop photo
QLQ workshop — QLQ workshop photo

Reference table

Vendor scriptProblemCounter
"3 months guaranteed"undefined testdemand a salt-spray / artificial-sweat tier instead
"Depends on personal use"refusing liabilityput acceptance test conditions in the contract
"All real-gold plating is fine"process tiers differ hugelyspecify the route (e.g., PVD white gold)
Supplier promised 3-month color retention, got 1 month - QLQ workshop photo
Process close-up — QLQ workshop photo

How we handle it on the line

  • The buyer's real question: how to verify BEFORE ordering?
  • Definitions: color retention = how long plating keeps hue/gloss; drivers = plating route (palladium vs cyanide bath vs PVD white-gold differ hugely), base material, use environment; there is no industry-standard "months" test — only proxy tests like salt spray and artificial perspiration.
  • Options — a verifiable pre-order kit: 1) specify the plating route and thickness tier; 2) agree proxy tests (artificial perspiration ISO 3160-2 / salt-spray tier) and pass criteria; 3) keep sealed reference samples and compare batches against them.
  • QLQ avoids "months" promises entirely: we quote "plating system + proxy-test tier + sealed-sample comparison per batch" — jewelry/hardware clients running this flow have eliminated the two-week-tarnish complaint class.
  • Ask: 1) which process route does this price buy?
  • 2) will you put test conditions in the contract?

Honest boundaries

  • 3) how is the sealed-sample system executed?
  • Honest boundary: every process has real limits (sweat, cosmetics, sea salt accelerate fading); we give tiers, not romantic numbers.
  • Next step: tell QLQ the target wear scenario (skin contact / daily wear / salty-humid); we reply with a route + test plan.

FAQ

Can QLQ provide test reports with the delivery?
Yes — salt spray, thickness and adhesion reports are attached per lot on request.
Can QLQ provide test reports with the delivery?
Yes — salt spray, thickness and adhesion reports are attached per lot on request.
Can QLQ provide test reports with the delivery?
Yes — salt spray, thickness and adhesion reports are attached per lot on request.