Scope of this guide

This junior-level guide sticks to the basics you must run without help: safe settings, daily checks and the pass criteria you can verify yourself.

Process: Mould Maintenance. Figures in this guide are industry-standard starting ranges; confirm against your supplier TDS before locking settings.

Working ranges and control points

The table below is the daily reference for a mould shop. Set by the card, verify by the control point column.

ParameterTypical rangeControl pointWatch out
Try-out shot count20–50 shots per tryDimensional first-articleJudge on stable shots only
Vent depth0.01–0.03 mm zincVent impression checkDeep vents flash heavy
Polish directionAlong ejectionRa reading at gatesCross polish drags filling
Cooling flowTurbulent, per circuitFlow meter per circuitLaminar flow warps parts
Slide clearancePer die spec ±0.02Blue-check slidesWear makes mismatch flash

Standard routine

  1. Clean cores with soft tools — steel scratches vent lands
  2. Blue-check slides at every service
  3. Log flow per cooling circuit at each pull
  4. Photograph vent lands after cleaning
  5. First-article dimension after every repair
Mould Maintenance junior - Live line operation - QLQ workshop photo
Live line operation — QLQ workshop photo

Engineer notes

  • Most flash is slide or parting-line wear, not clamp tonnage
  • Vent maintenance beats injection-speed tuning for porosity
  • Cooling balance decides warp; one clogged circuit hides in averages
  • Polish marks copy onto castings — polish along ejection
  • Spare cores for the two hottest cavities save the most downtime
Safety: Mould handling needs rated slings and clear floors. A dropped insert is a scrapped tool and a foot injury.
Mould Maintenance junior - Close-up of the working zone - QLQ workshop photo
Close-up of the working zone — QLQ workshop photo

FAQ

Where should I look first when flash appears?
Parting line and slides with a blue check — wear shows before dimension drift.
How often should vents be cleaned?
Every 10–20k shots for zinc, sooner with hot runner gates.
Why does one cavity warp parts?
Its cooling circuit is partly blocked; flow-meter each circuit, not just the inlet.