Scope of this guide

This junior-level guide sticks to the basics you must run without help: safe settings, daily checks and the pass criteria you can verify yourself.

Process: Pre-treatment & Cleaning. Figures in this guide are industry-standard starting ranges; confirm against your supplier TDS before locking settings.

Working ranges and control points

The table below is the daily reference for a cleaning line. Set by the card, verify by the control point column.

Stage / parameterTypical rangeControl pointWatch out
Alkaline soak cleaner40–60 g/L, 55–70 °CTitration 2× per shiftOil layers shorten bath life
Soak time3–8 minVisual water-break-freeUnder-clean hides under wax
Rinse 1 (counter-flow)TDS < 5000 ppmOverflow checked hourlyDrag-in salts to next tank
Acid activate, 10–20%30–60 sBright, uniform etchOver-etch on brass
Rinse after acidConductivity < 100 µS/cmBefore every plating tankChloride carry-over pits nickel

Standard routine

  1. Titrate cleaner bath at shift start
  2. Rack parts to avoid pockets that trap solution
  3. Observe water-break test after rinse
  4. Check acid bath strength before activation
  5. Record tank temps and concentrations in the log
Pre-treatment & Cleaning junior - Live line operation - QLQ workshop photo
Live line operation — QLQ workshop photo

Engineer notes

  • Water-break-free surface is the pass criterion — droplets must sheet, not bead
  • Counter-flow rinsing halves water use at the same cleanliness
  • Replace cleaner before oil carry-over reaches the soak tank walls
  • Acid activation time doubles for aged brass — adjust by visual etch
  • Never let parts dry between stages; re-soak instead
Safety: Mixing acids and alkalis in the wrong order can splash hot solution. Add chemicals to water, never water to chemicals, and wear face protection.

FAQ

What is the fastest check that cleaning worked?
The water-break test: rinse and hold the part vertically; film should sheet without beads.
Why do parts flash-rust after rinse?
Rinse water is contaminated or dwell before plating is too long. Increase overflow and shorten transfer.
How often should cleaner baths be titrated?
At least twice per shift, plus after any heavy oil load.