Painting Workshop — trades and people
This workshop covers 6 trades. Open any trade to see the level guide, or jump straight to the level you hire or train for. Each trade page carries the equipment scene, the parameters and the mistakes that matter at that level.
Search by trade + level (barrel senior), by defect (blistering), or by parameter (brightener dosing). Full-text and title search across the whole site.

Trades in this workshop
Rack Painting
Level guide →
Core trade of this workshop
E-Coating
Level guide →
Core trade of this workshop
Powder Coating
Level guide →
Core trade of this workshop
Cold Painting
Level guide →
Core trade of this workshop
Tumble Painting
Level guide →
Core trade of this workshop
Resin Dripping
Level guide →
Core trade of this workshop
How the four levels are judged

- Junior (1-3 yrs) — Runs the SOP, reads the parameter sheet, spots common defects
- Intermediate (3-5 yrs) — Knows why a parameter moves, reads data, diagnoses root causes
- Senior (5-8 yrs) — Owns the process window and the link to upstream/downstream steps
- Management (8+ yrs) — Cost, yield, rescue plans, team and customer communication
Not sure where a topic sits? Use the trade + level picker, or open the full knowledge map. Owners can start from the process overview.
Painting line types and when each fits
| Type | Output | Colour changes | Film consistency |
|---|---|---|---|
| Manual booth | Low to medium | Fast | Operator dependent |
| Automatic line | High | Slow (cleaning) | Consistent per fixture |
| Barrel / tumble | High for small parts | Slow | Even, but edge wear |
| Dip / resin drip | Medium | Fast | Drip marks on vertical faces |
Curing: the stage that decides durability
| Method | Typical condition | Watch |
|---|---|---|
| Air dry | Ambient, 30-60 min tack free | Adhesion improves over 24 h - do not pack early |
| Low bake | 60-80 C, 20-40 min | Heat-sensitive plastics distort |
| Standard bake | 120-160 C, 20-30 min | Colour shift on some pigments |
| UV cure | Seconds under lamp | Shadows in recesses stay wet |
FAQ
Why does the same colour look different on two lines?
Film build and substrate colour. Measure both before changing the paint.
How do we reduce paint consumption?
Fixture design and gun distance. Both are free to change compared with buying new equipment.
Related pages
FAQ
What about painting workshop — trades and people?
This workshop covers 6 trades. Open any trade to see the level guide, or jump straight to the level you hire or train for.
What about trades in this workshop?
Rack Painting Core trade of this workshop Level guide → Spray booth + hanging line Junior 3+ years (qualified technician) articles: 8 Intermediate 5+ years, solves 1-3 problem areas alone articles: 21 Senior 8+ years, covers most problems and trains others articles: 9 Management 5+ years, full trade coverage and t
How the four levels are judged?
How the four levels are judged - Years on the tools, plus what the person can actually run alone. Junior (1-3 yrs) — Runs the SOP, reads the parameter sheet, spots common defects Intermediate (3-5 yrs) — Knows why a parameter moves, reads data, diagnoses root causes Senior (5-8 yrs) — Owns the process window and the li
What about painting line types and when each fits?
Type Output Colour changes Film consistency Manual booth Low to medium Fast Operator dependent Automatic line High Slow (cleaning) Consistent per fixture Barrel / tumble High for small parts Slow Even, but edge wear Dip / resin drip Medium Fast Drip marks on vertical faces